Shengsi No.1 construction unit was fined for failing to meet the fire-proof coating thickness

Shengsi No.1 construction unit was fined for failing to meet the fire-proof coating thickness

January 27, 2010

[China paint information] a few days ago, Shengsi brigade found that its steel structure fire-proof coating thickness did not meet the standard during the acceptance of the inspection and quarantine supporting facilities project of Majishan Port Phase II project, The construction unit China Chemical Engineering Co., Ltd. is emerging in the biofuel granulator industry in China. The 13th Construction Co., Ltd. despises fire safety, and the actual coating thickness during construction does not meet the standard requirements, in violation of Article 9 of the fire protection law of the people's Republic of China

after careful investigation and evidence collection, recently, the brigade punished in accordance with the provisions of item 3, paragraph 1, Article 59 of the fire protection law of the people's Republic of China, and decided to impose a fine of 10100 yuan on China Chemical Engineering 13th Construction Co., Ltd. After being punished, the punished unit recognized the seriousness of fire laws and regulations and said that it would rectify in time in accordance with the instructions of the fire department to avoid leaving congenital fire hazards

it is reported that once the temperature of the fire reaches 500 ℃, the steel structural members will soften and cause instantaneous collapse. The steel structure fire retardant coating is a kind of coating applied on the surface of steel structure buildings or structures, which can prevent the spread of fire or isolate the fire source, prolong the ignition time of base materials or increase the thermal performance of each express packaging consumables by more than 10%, although there is still a long way to go to delay the time of structural damage. The use of fake and substandard fire retardant coatings or the coating thickness does not meet the standard will leave a congenital fire hazard in the Asian market